Academic publishing in Europe and N. America

Archive Publication ethics Submission Payment Contacts
In the original languageTranslation into English

Carbon - Carbon Composite Materials

Authors

Mykyta Liakh

Rubric:Technical sciences in general
2
0
Quote
2
0

Annotation

This article examines the application of carbon composite materials in the manufacture of three-dimensional porous electrode bodies, cathodes for electrochemical reactors intended for electrocoagulation, and flexible, permeable, non-metallic contacts.
For the manufacture of three-dimensional porous electrode bodies, it is proposed to use so-called carbon wool produced by UKRUGLECOMPOSITE in Ukraine. This material is manufactured as a nonwoven material in the form of sheets of varying thickness, ranging from 3 to 6 mm. These sheets can be stacked to achieve any required thickness and can readily assume the desired geometric shape under external pressure. According to the manufacturer, the active working surface area of this material is 100,000 times greater than that of other materials used for electrode manufacturing. The material is relatively inexpensive and can be easily disposed of, including by combustion in the open air or in furnaces.
For the manufacture of cathodes in electrochemical reactors intended for electrocoagulation, it is proposed to use a rigid composite material made from several layers of composite fabric additionally saturated with carbon through multistage pyrolysis under vacuum conditions. This manufacturing method also enables the production of tubes. Such a tube is proposed for use as a cathode. This cathode is completely resistant to corrosion, and its surface does not require passivation. The operational efficiency of the electrochemical coagulation reactor is significantly increased due to the aforementioned properties of the composite cathode.
For the manufacture of flexible, permeable, non-metallic contacts, it is proposed to use carbon composite fabric produced by UKRUGLECOMPOSITE in Ukraine under the name ETAN. This fabric has a viscose base saturated with carbon during multistage pyrolysis under vacuum conditions. The electrical resistance of the fabric is equivalent to that of steel, resulting in minimal energy losses during operation of the electrode cell. The fabric exhibits exceptional mechanical strength and chemical resistance. The maximum temperature at which the fabric retains its properties is 4,000°C.

Authors

Mykyta Liakh

Rubric:Technical sciences in general
2
0

Share

2
0

Other articles of the issue

Khurshida Davletova, Alisher Khaitbayev, Dilshod Mansurov Preparation and Comprehensive Characterization of an Aldehyde-Modified Hyaluronate-Containing Polysaccharide Fraction for Hydrogel Systems
85 views
cc-license
About us Journals Books
Publication ethics Terms of use of services Privacy policy
Copyright 2013-2025 Premier Publishing s.r.o.
Praha 8 - Karlín, Lyčkovo nám. 508/7, PSČ 18600, Czech Republic pub@ppublishing.org